I purchased most of the items I will need earlier this week, but it has been very cold so no work has been done. Still a lot of paint to get off.
A cold smoker might be ok , but in my opinion it not worth the effort, when you finish, you still have an old fridge
Glass bead blasting is not a good media for paint removal.Black Beauty,aka ground slag is though.
Had a reaction where the black paint I just put on and the red paint over primer I put on a week ago suddenly wrinkled and can whipe down to bar metal again. Anyone know the cause? I've ran into this before when painting electrical boxes at work with multiple layers of paint, always thought it was because the first layer wasn't dry or the metal wasn't roughed enough.
Also I cut this by making a stencil from cardboard tracing of opening in SFB, then cutting with jigsaw. First cut I tried with tin snips, workes but jagged crappy opening. Looks much better with jigsaw cut.